Plastics. Differential scanning calorimetry (DSC) - Determination of glass transition temperature and step height

Plastics. Differential scanning calorimetry (DSC) - Determination of glass transition temperature and step height

Regular price
£134.00
Sale price
£134.00
Regular price
£67.00
Sold out
Unit price
per 

1   Scope

This document specifies methods for the determination of the glass transition temperature and the step height related to the glass transition of amorphous and partially crystalline plastics.